HSLA
High Strength Low Alloy
Product | GS80 | GS125 | GS150 |
Min. YS | 80 KSI | 125 KSI | 150 KSI |
Typical YS | 90 KSI | 125-135 KSI | 150-160 KSI |
Typical UTS | 100 KSI | 125-135 KSI | 160-170 KSI |
Typical Elong. | 18% min. | 2% min. | 1.5% min. |
Typical Hardness | 90 Rb Min. | 95-105 Rb | 29-33 Rc |
Approximate values – inside bending radius
Bend | GS80 | GS125 | GS150 |
90° Transverse | 1T | 1 to 3T | 1 to 3T |
GS80 | 0.020″ to 0.165″ |
GS125 | 0.015″ to 0.150″ |
GS150 | 0.015″ to 0.125″ |
Standard HSLA products are available in strength ranges varying from 35ksi min yield to 80ksi min yield.
HSLA | Grade 35 | Grade 50 | Grade 60 | Grade 80 |
Yield | 35 ksi min | 50 ksi min | 60 ksi min | 80 ksi min |
Tensile | 45 ksi min | 60 ksi min | 70 ksi min | 90 ksi min |
Elongation | 22% min | 20% min | 18% min | 12% min |
Grade | 1008/1010 5 temper | 1008/1010 3 temper | 1008/1010 1 temper | 1050 Annealed | 1050 Full Hard |
Yield | 24-35 ksi | 35-45 ksi | 64-84 ksi | 43-55 ksi | 100-110 ksi |
Tensile | 38-50 ksi | 45-65 ksi | 80-100 ksi | 65-75 ksi | 110-120 ksi |
Elongation | 33-45% | 13-27% | 1-5% | 19-28% | 3-6% |